Assessing Mixing Quality of a Copovidone-TPGS Hot Melt Extrusion Process with Atomic Force Microscopy and Differential Scanning Calorimetry
Journal Title: AAPS PharmSciTech - Year 2016, Vol 17, Issue 1
Abstract
Atomic force microscopy (AFM) and modulated differential scanning calorimetry (mDSC) were used to evaluate the extent of mixing of a hot melt extrusion process for producing solid dispersions of copovidone and D-α-tocopherol polyethylene glycol 1000 succinate (TPGS 1000). In addition to composition, extrusion process parameters of screw speed and thermal quench rate were varied. The data indicated that for 10% TPGS and 300 rpm screw speed, the mixing was insufficient to yield a single-phase amorphous material. AFM images of the extrudate cross section for air-cooled material indicate round domains 200 to 700 nm in diameter without any observed alignment resulting from the extrusion whereas domains in extrudate subjected to chilled rolls were elliptical in shape with uniform orientation. Thermal analysis indicated that the domains were predominantly semi-crystalline TPGS. For 10% TPGS and 600 rpm screw speed, AFM and mDSC data were consistent with that of a single-phase amorphous material for both thermal quench rates examined. When the TPGS concentration was reduced to 5%, a single-phase amorphous material was achieved for all conditions even the slowest screw speed studied (150 rpm).
Authors and Affiliations
Matthew S. Lamm, James DiNunzio, Nazia N. Khawaja, Louis S. Crocker, Anthony Pecora
An Investigation into the Effect of Fine Lactose Particles on the Fluidization Behaviour and Aerosolization Performance of Carrier-Based Dry Powder Inhaler Formulations
The effect of milled and micronized lactose fines on the fluidization and in vitro aerosolization properties of dry powder inhaler (DPI) formulations was investigated, and the suitability of static and dynamic methods fo...
Hydrogels Composed of Cyclodextrin Inclusion Complexes with PLGA-PEG-PLGA Triblock Copolymers as Drug Delivery Systems
Although conventional pharmaceuticals have many drug dosage forms on the market, the development of new therapeutic molecules and the low efficacy of instant release formulations for the treatment of some chronic disease...
Development of Duloxetine Hydrochloride Loaded Mesoporous Silica Nanoparticles: Characterizations and In Vitro Evaluation
The online version of this article (doi:10.1208/s12249-014-0273-x) contains supplementary material, which is available to authorized users.
Development, Optimization, and Characterization of PEGylated Nanoemulsion of Prostaglandin E1 for Long Circulation
Lipo-PGE1 is the most widely used formulation of PGE1 in clinic. However, PGE1 is easier to leak out from lipo-PGE1 and this will lead to the phlebophlogosis when intravenous injection. The stability of lipo-PGE1 in stor...
Drug in Adhesive Patch of Zolmitriptan: Formulation and In vitro/In vivo Correlation
The objective of the present study was to develop transdermal patch for zolmitriptan, determine its in vivo absorption using the rabbit skin. Solvent evaporation technique prepared zolmitriptan patch was settled in two-c...