Abstract
In the aerospace industry, passenger safety depends on proper quality control at each production stage. The main responsibility for the correct operation of the aircraft lies within a gas turbine. A proper and rigorous selection of the gas turbine construction material is required, and in a further step, the method of joining the construction parts. Nickel superalloys due to the high heat resistance, strength and creep resistance at high temperatures, toughness and corrosion resistance, are very often used for the construction of a gas turbine engine. In the next step, the selection of joining method is necessary. This method must be able to achieve high-quality connections, resistant to work at high temperatures and corrosive environments. The most effective bonding method that meets the above conditions is brazing. In this study non-destructive (visual) test and destructive (metallographic) test of brazed joint of Inconel 718 and Inconel 625 were conducted.<br/><br/>
Authors and Affiliations
Katarzyna Strzelczak, Barbara Lisiecka
Analysis of information security threats for developing DLP-systems
The motivation of investigation is explained by the problem of keeping organisations’ information and private ones secure. One reason for this is insufficiency of information protection systems, and another – vulnerabili...
Work safety in production processes located in Poland
This article presents selected aspects connected to work safety, related to production facilities in Po-land, where production lines are installed as new, or transferred from other locations. The author fo-cuses on ensur...
Value Stream Mapping as Lean Production tool to improve the production process organization – case study in packaging manufacturing
In the paper, the method of the production process improvement with the use of lean production tools has been presented. The Value Stream Mapping (VSM) for the cardboard packaging produc-tion process has been presented....
LEAN Production issues in the organization of the company - results
The key to the functioning of enterprises in today's market is the concept of flexibility, which is mainly associated with adapting to very dynamically changing customer requirements. The basis for this ap-proach is, amo...
Mechanical and mathematical research of local deformations of a steel roller shell with a variable geometry of contact surface
The article is devoted to solving the fundamental and applied problem of nonlinear structural mechanics of machines by introducing into the drum two additional stop cylinders with supporting rollers at the end and adjust...