Abstract

Purpose: This article describes preparation and characterization of beads of alginate containing probiotic bacteria of Lactobacillus acidophilus DMSZ20079. Methods: Fourteen formulations using different alginate (ALG) and CaCl2 concentrations as well as hardening times were prepared using extrusion technique. The prepared beads were characterized in terms of size, morphology, encapsulation efficiency and bacterial viabilities in acid (pH 1.8, 2 hours) condition. Results: The results showed that spherical beads with narrow size distribution ranging from 1.32±0.04 to 1.70±0.07 mm were achieved with encapsulation efficiency higher than 98%. Surface response analysis revealed that alginate concentration was the important factor for the size, shape and encapsulation efficiency of prepared beads. Furthermore, survived bacteria after acid exposure in all prepared beads (63-83%) were significantly higher than those of untreated cells (39%) and enhanced by increasing alginate concentration. Surface response analysis revealed that the effect of all three factors of alginate and CaCl2 concentrations as well as hardening times were significant in acid viability, however alginate concentration played the most important role according to its regression coefficient. Conclusion: Among alginate and CaCl2 concentrations as well as hardening times, alginate concentration was the most variable in the characteristics of Alginate beads.

Authors and Affiliations

Farzaneh Lotfipour, Shahla Mirzaeei, Maryam Maghsoodi

Keywords

Related Articles

Comparison of in Vitro Activity of Doripenem versus Old Carbapenems against Pseudomonas Aeruginosa Clinical Isolates from both CF and Burn Patients

Purpose: The antimicrobial activity of doripenem in comparison of imipenem, meropenem and ertapenem among Pseudomonas aeruginosa isolated from burn and Cystic Fibrosis (CF) patients were determined. Methods: Metallo-β-la...

Association between Thrombophilia and Repeated Assisted Reproductive Technology Failures

Purpose: This study was performed to investigate the incidence of thrombophilic gene mutations in repeated assisted reproductive technology (ART) failures. Methods: The prevalence of mutated genes in the patients with a...

Dose-Dependent Effect of Flouxetine on 6-OHDA-Induced Catalepsy in Male Rats: A Possible Involvement of 5-HT1A Receptors

Purpose: Progressive loss of dopaminergic neurons of the substantia nigra pars compacta (SNc) in Parkinson’s disease (PD) leads to impairment of motor skills. Several evidences show that the role of serotonergic system i...

Antioxidant and Antimicrobial activity of Pedicularis sibthorpii Boiss. And Pedicularis wilhelmsiana Fisch ex.

Purpose: This research paper presents antioxidant and antimicrobial activities of Pedicularis sibthorpii and Pedicularis wilhelmsiana which grow in Azerbaijan/Iran with claimed a lot of therapeutic effects. Methods: DPPH...

Targeted Fluoromagnetic Nanoparticles for Imaging of Breast Cancer MCF-7 Cells

Purpose: To achieve simultaneous imaging and therapy potentials, targeted fluoromagnetic nanoparticles were synthesized and examined in human breast cancer MCF-7 cells. Methods: Fe3O4 nanoparticles (NPs) were synthesized...

Download PDF file
  • EP ID EP135467
  • DOI 10.5681/apb.2012.010
  • Views 99
  • Downloads 0

How To Cite

Farzaneh Lotfipour, Shahla Mirzaeei, Maryam Maghsoodi (2012). Evaluation of the effect of CaCl2 and alginate concentrations and hardening time on the characteristics of Lactobacillus acidophilus loaded alginate beads using response surface analysis. Advanced Pharmaceutical Bulletin, 2(1), 71-78. https://europub.co.uk./articles/-A-135467