Exploitation of Nanoindentation and Statistical Tools to Investigate the Behavior of Materials
Journal Title: Engineering, Technology & Applied Science Research - Year 2016, Vol 6, Issue 4
Abstract
The determination of the performance of materials requires the characterization of materials at scales: macro, micro and nanoscale. Among the most common experimental methods one can find the instrumented indentation test for determining the contact stiffness and contact depth and analyzing the characteristic curve by nanoindentation load on the penetration of the indentor. Through statistical processing of the experimental results, the rigidity of contact on the contact depth is investigated, depending on the indentation load, for bronze, brass and copper. A mathematical model is adopted to describe the polynomial regression by the method of least squares growth rigidity with one or more geometric parameters representative of the size of the footprint. This study allows us to identify factors that influence the rigidity of the materials examined and the sensitivity of the used indenters.
Authors and Affiliations
L. Aminallah, S. Habibi
A Review of Two Nanocomposite Insulating Materials Models: Lewis’ Contribution in the Development of the Models, their Differences, their Similarities and Future Challenges
Nanocomposite polymers are nowadays a major field of research. This paper investigates the interpretational possibilities of two models developed, namely, Tsagaropoulos’ model and Tanaka’s model. Particular emphasis is g...
Design Practices in Harmonic Analysis Studies Applied to Industrial Electrical Power Systems
Power system harmonics may cause several problems, such as malfunctions of electrical equipment, premature equipment failures and plant shutdowns. Accordingly, mitigation of these harmonics is considered an important tar...
A Review on Energy Efficient CMOS Digital Logic
Autonomy of power supply used in portable devices directly depends on energy efficiency of digital logic. This means that digital systems, beside high processing power and very complex functionality, must also have very...
Leakage Reduction in Water Distribution Systems with Efficient Placement and Control of Pressure Reducing Valves Using Soft Computing Techniques
Reduction of leakages in a water distribution system (WDS) is one of the major concerns of water industries. Leakages depend on pressure, hence installing pressure reducing valves (PRVs) in the water network is a success...
Effect of Standard No. 2800 Rules for Moment Resisting Frames on the Elastic and Inelastic Behavior of Dual Steel Systems
According to most valid Design Codes including the Iranian Seismic Design Code (Standard No. 2800), moment resisting frames in dual systems must have the ability of resisting the 25% of the total lateral load of the dual...