Influence analysis foamed polystyrene model on casting defects as well as microstructure ductile cast iron from Lost Foam process with Inmold method
Journal Title: Archiwum Odlewnictwa - Year 2011, Vol 11, Issue 3
Abstract
In this work was shown a influence analysis foamed polystyrene model on casting defects as well as microstructure ductile cast iron from Lost Foam process with Inmold method.
Authors and Affiliations
P. Just, T. Pacyniak
Preliminary Research on Granulation Process of Dust Waste from Reclamation Process of Moulding Sands with Furan Resin
The results of investigations of the granulation process of foundry dusts generated in the dry mechanical reclamation process of used sands, where furan resins were binders are presented in the paper. Investigations conc...
Analysis of power demand signal in laboratory rotary mixer
The paper summarises the power measurement data for the main assemblies in a prototype turbine mixers for laboratory applications. Of particular interest are power demand signals in the paddle stirrer and the rotor. Test...
Ecological aspects of the use of lost foam patterns
The paper discusses some aspects of ecology in the use of lost foam patterns for piece production of large castings poured from ferrous alloys under the conditions of Metalodlew SA. Foundry. The technological processes u...
Moulding Sands with New Inorganic Binders - Ecology Assessment in the Aspect of Work Environment
The development of economy and industry introducing new technologies and materials often means the increased threat of occurrence of factors harmful to humans and environment. Workers employed in foundries as mould poure...
Assessment Criteria of Bentonite Binding Properties
The criteria, with which one should be guided at the assessment of the binding properties of bentonites used for moulding sands, are proposed in the paper. Apart from the standard parameter which is the active bentonite...