Abstract

Aluminium coating due to its ability to form stable alumina oxide scale are commonly used to protect materials such as inconel 718 superalloys at high operational temperatures. Relevant properties of the oxide scale formed; growth rate and coating adherence is not only determined by the composition of the coating material used but is also influenced by the coating manufacturing process and the test condition. In the present work, effect of water vapour and thermocycling commonly prevailing on the morphology and composition of the alumina scales formed during high temperature oxidation was studied using hot-dip and plasma spray aluminium coatings. The coatings highly improved oxidation resistance of the alloy substrate with hot dip coating showing the lowest mass change compared to plasma spray. The results also show that the hot-dip coating has an inherently different morphology and growth rate compared to those formed on the plasma spray coating. High rate of oxidation, spallation and large voids with little protective alumina oxide layer were observed in moist condition test especially in plasma spray coatings.

Authors and Affiliations

Pius Kibet KOECH, Chaur Jeng WANG

Keywords

Related Articles

Enhanced Magnetic Squareness in Manganese-Bismuth Mechanical Alloys Incorporating Magnesium Oxide

Manganese-bismuth (MnBi) mechanical alloys have been under development for novel permanent magnets without rare-earth elements. The ball-milling of bismuth (III) oxide and manganese powders in this work leads to soft mag...

Effect of Er Addition on the High Temperature Strength of Al-Si-Cu-Ni-Mg-Fe Piston Alloys by T5 and T6 Heat Treatment

In this study, the dependence of Er addition (0 – 0.49 wt.%) on the microstructural evolution and related tensile strength at high temperature (HT) were investigated for the eutectic Al-Si piston alloys. The results show...

The Effect of Nanoparticle Surface State on Trap Level Distribution of Polyimide/Aluminum Nitride-montmorillonite Nanocomposite Films

The electrical properties of polyimide (PI) nanocomposites, which are widely used in microelectronic industry and electrical engineering fields, strongly depend on the surface state of nanoparticles. To explore this depe...

A Novel Approach for Accelerated Fabrication of Calcium Hydroxyapatite Thin Films

In this study we demonstrate, that sol–gel route is suitable to quicker obtain calcium hydroxyapatite (Ca10(PO4)6(OH)2, CHAp) coatings on crystalline Si substrate by modified dip-coating technique. The substrate was dip-...

Synthesis, Characterization of Metal-Schiff Base Functionalized Mesoporous Silica for Pesticide Adsorption

The mesoporous silica modified by salicylaldimine was prepared through a co-condensation method. Through the bridge effect from metal ion (copper ion, zinc ion, manganese ion), the model drug-avermectin was supported on...

Download PDF file
  • EP ID EP674917
  • DOI 10.5755/j01.ms.25.4.21334
  • Views 61
  • Downloads 0

How To Cite

Pius Kibet KOECH, Chaur Jeng WANG (2019). Performance Characteristics of Hot-dip and Plasma Spray Aluminide Coated Nickel-Based Superalloy 718 under Cyclic Oxidation in Water Vapour. Materials Science-Medžiagotyra, 25(4), 413-421. https://europub.co.uk./articles/-A-674917