Abstract

Nanoindentation is usually applied on thin films at ambient temperatures for hardness determination. Recently, instruments for conducting nanoindentation at elevated temperatures have been developed facilitating measurements up to 700 oC. Both indenter and specimen, if necessary, are heated in an inert atmosphere to avoid film oxidations. In the described investigations, nanoindentations were conducted on cemented carbides and high speed steel specimens, coated with various films, up to 400 oC. The obtained results were subjected to statistical analysis to estimate their reliability. Moreover, the results were evaluated by appropriate FEM (Finite Element Method) algorithms for determining the coatings’ elasticity modulus, yield and rupture stress as well as hardness at various temperatures. The results reveal a non-linear temperature dependence of the coating properties.

Authors and Affiliations

K. -D. Bouzakis, M. Pappa, S. Gerardis, G. Skordaris, E. Bouzakis

Keywords

Related Articles

Effect of Band Contact on the Temperature Distribution for Dry Friction Clutch 

In this study, the two dimensional heat conduction problem for the dry friction clutch disc is modeled mathematically analysis and is solved numerically using finite element method, to determine the temperature field whe...

Recycled Aluminium Cans/Eggshell Composites: Evaluation of Mechanical and Wear Resistance Properties

Aluminium based metal matrix composites have been produced from recycled aluminium cans and 150µm sized eggshell particles using a stir cast process. The mechanical properties of the control and aluminium can/eggshell co...

Tribological and Wear Properties of Multi-Layered Materials

The usage of fabrics as reinforcements in composites is spreading due to fabrics’ properties. The use of fabrics allows obtaining of sinuous surfaces, for instance, unlike the use of prepregs. Using fabrics as reinforcem...

Studies on Mechanical Behaviour of Aluminium/Nickel Coated Silicon Carbide Reinforced Functionally Graded Composite

The aim of the work is to fabricate functionally graded aluminium (Al-Si6Cu)/ nickel coated SiC metal matrix composite using centrifugal casting route. SiC particles (53-80 µm) were coated with nickel using electroless c...

Study of Wear and Friction of Al-Fe Metal Matrix Composite Produced by Liquid Metallurgical Method

A modified impeller mixing coupled with chill casting technique was used for the preparation of Al-Fe composite. The electrolytic grade iron powder of 300mesh size was dispersed in the melt of commercially pure aluminum....

Download PDF file
  • EP ID EP108654
  • DOI -
  • Views 96
  • Downloads 0

How To Cite

K. -D. Bouzakis, M. Pappa, S. Gerardis, G. Skordaris, E. Bouzakis (2012). PVD Coatings’ Strength Properties at Various Temperatures by Nanoindentations and FEM Calculations Determined. Tribology in Industry, 34(1), 29-35. https://europub.co.uk./articles/-A-108654